Product
Permanent magnetism in phosphine
Permanent magnetism in phosphine- and chlorine-capped gold: from clusters to nanoparticles
Magnetometry results have shown that gold NPs (∼2 nm in size) protected with phosphine and chlorine ligands exhibit permanent magnetism. When the NPs size decreases down to the subnanometric size range, e.g. undecagold atom clusters, the permanent magnetism disappears. The near edge structure of the X-ray absorption China magnets spectroscopy data points out that charge transfer between gold and the capping system occurs in both cases. These results strongly suggest that nearly metallic Au bonds are also required for the induction of a magnetic response. Electron paramagnetic resonance observations indicate that the contribution to magnetism from eventual iron impurities can be disregarded.
- EMAILsales@china-magnet.net ICP:05020812
- TEL: 0086-592-5781916 5144899 FAX: 0086-592-5123653
- ADD: Unit H, 4F Rihua Mansion,No. 8 Xinfeng 2nd road,Torch Hi-Tech Zone,Xiamen,China.
- Copyright @ Xiamen Everbeen Magnet Electron Co.,Ltd. All Right Reserved.
- neodymium magnets| permanent magnet |alnico magnet |Neodymium magnet|ceramic magnet| samarium cobalt magnet|Refrigerator Magnet|rare earth magnet